Standard Practice for Cutting Film and Sheeting Test Specimens


Importancia y uso:

3.1 Many test methods including Test Methods D882, D2838, F88/F88M, F1921/F1921M, and F2029 require the use of narrow strips of varying length. The quality of the sample preparation directly affects test results. This practice describes three techniques for preparing samples with straight, clean, parallel edges with no visible imperfections.

Note 2: After cutting, each specimen should be examined visually to ensure the edges are undamaged (free of nicks). On a periodic basis specimen edge quality should be evaluated by microscopic examination. To determine when cutting blades need to be replaced or sharpened, a control chart of tensile strength and percent elongation at break (see Test Method D882) of a uniform material may be maintained. Tensile strength and percent elongation at break will decrease as the quality of specimen cutting decreases.

Subcomité:

D20.19

Referida por:

D2838-18, D6988-21, D6988-21, D6988-21, D0882-18, D0882-18, D0882-18, D0882-18

Volúmen:

08.03

Número ICS:

25.100.01 (Cutting tools in general)

Palabras clave:

film; sample preparation; sheeting;