Standard Guide for Hot Isostatic Pressing (HIP) of Aluminum Alloy Castings


Importancia y uso:

4.1 HIP of castings should be performed in the as cast condition. Post HIP inspection of castings should result in a reduction of porosity that is evident in x-ray grade and properties.

4.2 HIP will not eliminate inclusions or surface-connected porosity in a casting.

Subcomité:

B07.01

Volúmen:

02.02

Número ICS:

77.120.10 (Aluminium and aluminium alloys), 77.150.10 (Aluminium products)

Palabras clave:

aluminum casting; autoclave; densification; HIP; HIPing; hot isostatic pressing; internal voids; inert gases; porosity; pressure; thermal couple; thermal treatment;