Standard Test Method for Microscopical Analysis by Reflected Light and Determination of Mesophase in a Pitch


Importancia y uso:

5.1 Sometimes coal tar and petroleum pitches are heat treated thereby forming mesophase spheroids. The mesophase may be partially soluble in quinoline and cannot be estimated by the quinoline insoluble test (Test Method D2318). This test method provides for the identification, quantitative estimation, and size determination of mesophase spheroids.

5.2 The mesophase initially forms as spheroids that may coalesce to form a variety of asymmetrical shapes. The smallest mesophase particle that can be detected with certainty at 400× or 500× magnification is 4 μm in diameter; mesophase particles sizes less than 4 μm should be ignored. If mesophase material less than 4 μm in size is of interest, then magnifications of 1000× to 1800× shall be used and the results should be appropriately identified. This method is limited to determining minor levels of mesophase, that is, ≤20 % mesophase.

Subcomité:

D02.05

Volúmen:

05.02

Número ICS:

91.100.50 (Binders. Sealing materials)

Palabras clave:

cenospheres; mesophase; microscopy; optical; pitch; QI; quinoline;

$ 1,194

Agregar al carrito

Norma
D4616

Versión
23

Estatus
Active

Clasificación
Test Method

Fecha aprobación
2023-10-01