Standard Test Method for Failure End Point in Accelerated and Outdoor Weathering of Bituminous Materials


Importancia y uso:

4.1 The extent of cracking or pitting of bituminous films is a measure of the extent of deterioration due to weathering. Failure due to cracking is more accurately determined electrically than visually.

4.2 Failure determined by this test method will depend not only on the characteristics of the bituminous material and the extent of weathering, but also on the film thickness, and the amount and type of mineral filler present.

4.3 Tests on a similar material of known weathering characteristics (a control) exposed at the same time as the test material is strongly recommended as a check on the validity of the test results.

Subcomité:

D08.02

Referida por:

D4798_D4798M-11R21, D4799_D4799M-17R23

Volúmen:

04.04

Número ICS:

91.100.50 (Binders. Sealing materials)

Palabras clave:

accelerated weathering; bituminous materials; failure end point; outdoor weathering;