Standard Test Method for Longitudinal Measurement of Volume Resistivity for Extruded Crosslinked and Thermoplastic Semiconducting Conductor and Insulation Shielding Materials


Importancia y uso:

4.1 The electrical behavior of semiconducting extruded shielding materials is important for a variety of reasons, such as safety, static charges, and current transmission. This test method is useful in predicting the behavior of such semiconducting compounds. Also see Test Method D4496.

Subcomité:

D09.07

Referida por:

D3004-08R20

Volúmen:

10.02

Número ICS:

29.045 (Semiconducting materials), 29.060.01 (Electrical wires and cables in general)

Palabras clave:

conductor shield; conductor shielding material; insulation shield; insulation shielding material; moderately conductive; semiconducting shielding materials; semiconducting shields; volume resistivity of shielding materials;

$ 948

Agregar al carrito

Norma
D6095

Versión
12(2023)

Estatus
Active

Clasificación
Test Method

Fecha aprobación
2023-05-01