Standard Test Method for Thermal Stability of Way Lubricants


Importancia y uso:

5.1 Thermal stability characterizes physical and chemical property changes which may adversely affect an oil's lubricating performance. This test method evaluates the thermal stability of a way lubricant in the presence of copper and steel rods at 100 °C. Deposits and rod colors are the evaluation criteria. No correlation of the test to field service has been made.

5.2 This test method is intended for use in qualifying a way lubricant, rather than for quality control or condition monitoring purposes.

Subcomité:

D02.L0.01

Volúmen:

05.02

Número ICS:

75.100 (Lubricants, industrial oils and related products)

Palabras clave:

bed lubricants; Cincinnati Milacron; copper corrosion; deposits; heat test; oil sludging; slideway lubricants; steel corrosion; thermal stability; way lubricants;

$ 954

Agregar al carrito

Norma
D6203

Versión
22

Estatus
Active

Clasificación
Test Method

Fecha aprobación
2022-11-01